国外套管腐蚀检测技术研究进展

王丽忱, 甄鉴, 朱桂清

科技导报 ›› 2014, Vol. 32 ›› Issue (18) : 67-72.

PDF(1662 KB)
PDF(1662 KB)
科技导报 ›› 2014, Vol. 32 ›› Issue (18) : 67-72. DOI: 10.3981/j.issn.1000-7857.2014.18.011
综述文章

国外套管腐蚀检测技术研究进展

作者信息 -
1. 中国石油集团经济技术研究院, 北京 100724;
2. 中国石油集团渤海钻探工程有限公司第二钻井分公司, 廊坊 065007
作者简介:
王丽忱,工程师,研究方向为石油科技信息监测,电子信箱:wlcwayne@126.com

Review on Casing Corrosion Testing Techniques outside China

Author information -
1. CNPC Economics & Technology Research Institute, Beijing 100724, China;
2. No. 2 Drilling Company, CNPC Bohai Drilling Engineering Company Limited, Langfang 065007, China

摘要

油气勘探生产过程中普遍存在腐蚀现象,为防止套管、油管、井口等设施的利用价值受到影响,保障经济效益、生产效率,需要开展腐蚀防控工作。腐蚀检测技术具有分辨率高、连续性强等特点,是应对腐蚀问题的重要手段。本文主要针对套管腐蚀问题,介绍国外套管腐蚀检测技术现状,并分析其未来发展趋势。

Abstract

Corrosion phenomena are widespread during the process of oil and gas exploration and production. Corrosion prevention and control are necessary in protection of oil-gas exploitation facilities, such as the casing, tubing and wellhead, to guarantee economic and production efficiency. Corrosion testing techniques are important means to deal with corrosion problems with high resolution and good continuity. This paper mainly addresses the casing corrosion problems by introducing the current status and development trend of casing corrosion testing techniques outside China.

关键词

套管腐蚀 / 电磁 / 超声波 / 井下电视 / 机械井径测量

Key words

casing corrosion / electromagnetics / ultrasonic / downhole camera / mechanical caliper

引用本文

导出引用
王丽忱, 甄鉴, 朱桂清. 国外套管腐蚀检测技术研究进展[J]. 科技导报, 2014, 32(18): 67-72 https://doi.org/10.3981/j.issn.1000-7857.2014.18.011
WANG Lichen, ZHEN Jian, ZHU Guiqing. Review on Casing Corrosion Testing Techniques outside China[J]. Science & Technology Review, 2014, 32(18): 67-72 https://doi.org/10.3981/j.issn.1000-7857.2014.18.011
中图分类号: TE925   

参考文献

[1] Koch G H, Brongers M P H, Thompson N G, et al. Corrosion cost and preventive strategies in the united states[R/OL]. [2010-02-03]. http://www.corrosioncost.com/home.html.
[2] NACE. Monitoring corrosion in oil and gas production with iron counts[R/OL]. [2011-04-05]. http://www.setlaboratories.com/NACE/tabid/61/Default.aspx.
[3] Brill T M, Calvez J L L, Demichel C, et al. Electromagnetic casing inspection tool for corrosion evaluation[C]. International Petroleum Technology Conference, Bangkok, Thailand, February 7-9, 2012.
[4] Brondel D, Edwards R, Hayman A, et al. Corrosion in the oil industry[J]. Oilfield Review, 1994, 6(2), 4-18.
[5] Lord W, Sun Y S, Udpa S S, et al. A finite element study of the remote field eddy current phenomenon[J]. Magnetics, IEEE Transactions on, 1988, 24(1): 435-438.
[6] Kermani M B, Morshed A. Carbon dioxide corrosion in oil and gas production—A compendium[J]. Corrosion, 2003, 59(8): 659-683.
[7] Li S, Liu C, Shen L. A New 3-D electrode-type logging tool[C]. 2006 SEG Annual Meeting. Society of Exploration Geophysicists, New Orleans, USA, October 1-6, 2006.
[8] 孙喜寿. 井下套管腐蚀监测及评定多层套管柱腐蚀的解释技术[J]. 国 外石油工程,1993(1): 58-64. Sun Xishou. Downhole casing corrosion monitoring and evaluation of the interpretation of the multilayer casing corrosion technology[J]. Foreign oil engineering, 1993(1): 58-64.
[9] 杨旭, 刘书海, 李丰, 等. 套管检测技术研究进展[J]. 石油机械, 2013, 41(8): 17-22. Yang Xu, Liu Shuhai, Li Feng, et al. Research progress in casing detection technology[J]. China Petroleum machinery, 2013, 41(8): 17-22.
[10] 唐宇. 套管井分析技术ABC (Analysis Behind Casing)[J]. 测井技术, 2011, 35(1): 88. Tang Yu. Analysis behind casing[J]. Well logging technology, 2011, 35 (1): 88.
[11] 林俊明. 电磁无损检测技术的现状与发展趋势[C]//中英无损检测技 术研讨会论文集. 上海: 中国机械工程学会, 2005: 42-50. Lin Junming. The current situation and trend of development of electromagnetic nondestructive testing technology[C]//Nondestructive Testing Technology Symposium. Shanghai: Chinese Mechanical Engineering Society, 2005: 42-50.
[12] 关松. 油水井套损检测技术分析与评价[J]. 石油仪器, 2010, 24(2): 64-66. Guan Song. Oil and water wells casing damage detection technology analysis and evaluation[J]. Oil Instrument, 2010, 24(2): 64-66.
[13] 李福军, 陈月勋, 李晓川, 等. 油水井套管的腐蚀及防护理论、实验与 应用—油水井套管的腐蚀与防护[J]. 大庆石油学院学报, 2004, 28 (2): 57-62. Li Fujun, Chen Yuexun, Li Xiaochuan, et al. Corrosion and anticorrosion of casing in oil and water wells[J]. Journal of Daqing Petroleum Institute, 2004, 28(2):57-62.
[14] Zhu G Y, Zhang S C, Liang Y B, et al. Origins of high H2S-bearing natural gas in China[J]. Acta Geol Sinica, 2005, 79(5): 697-708.
[15] Yin Z F, Zhao W Z, Bai Z Q, et al. Corrosion behavior of SM80SS tube steel in stimulant solution containing H2S and CO2[J]. Electrochemica Acta, 2008, 53(10): 3690-3700.
[16] 王军, 毕宗岳, 张劲楠, 等. 油套管腐蚀与防护技术发展现状[J]. 焊 管, 2013, 36(7): 17-22. Wang jun, Bi Zongyue, Zhang Jinnan, et al. Current status of casing/tubing corrosion and protection technology[J]. Welded Pipe and Tube, 2013, 36(7): 17-22.
[17] Brill T M, Calvez J L L, Demichel C, et al. Quantitative corrosion assessment with an EM casing inspection tool[C]. SPE 149069, New Orleans, USA, May 15-18, 2011.
[18] Schlumberger Limited. Casing corrosion measurement to extend asset life[EB/OL]. [2013-10-03]. http://www. slb.com/-/media/Files/resources/oilfield_review/ors13/aut13/2_casing_corr.pdf.
[19] Schlumberger Limited. Scanning for downhole corrosion[EB/OL]. [2013-10-25]. http://www.slb.com/-/media/Files/resources/oilfield_review/ors 10/spr10/04_downholecorrosion.pdf.
[20] Schlumberger Limited. EM pipe scanner brochure[EB/OL]. [2013-07-1 3]. http://www.slb.com/-/media/Files/evaluation/brochures/scanner_rock_ fluid_character/em_pipe_scanner_br.pdf.
[21] Schlumberger Limited. METT multi-frequency electromagnetic thickness tool[EB/OL].[2013-06-09].http://www.slb.com/services/characterization/wireline_cased_hole/corrosion_evaluationmultifrequency_electromagnetic. aspx.
[22] Schlumberger Limited. UCI ultrasonic casing imager[EB/OL]. [2013-11-23]. http://www.slb.com/services/characterization/wireline_cased_hole/corrosion_evaluation/ultrasonic_casing_imager.aspx.
[23] 谢荣华, 刘继生, 张月秋, 等. 检查套管损坏的电磁探伤测井方法及 应用[J]. 测井技术, 2003(3): 69-72. Xie Ronghua, Liu Jisheng, Zhang Yueqiu, et al. Detecting casing damages with electromagnetic defect detection log and its applications[J]. Well logging technology, 2003(3): 69-72.
[24] Baker Hughes Limited. Well integrity service[EB/OL]. [2013-09-14]. http://www.bakerhughes.com/products-and-services/evaluation/casedhole-wireline-systems/well-integrity.
[25] Halliburton Limited. Casing integrity monitoring for mature fields[EB/OL]. [2013-12-11]. http://www.halliburton.com/public/lp/contents/Brochures/web/H010381.pdf.
[26] Halliburton Limited. XaminerTN multicomponent induction (MCI) tool[EB/OL]. [2013-02-08]. http://www.halliburton.com/public/lp/contents/Data_Sheets/web/H/H09310.pdf.
[27] Halliburton Limited. Downhole video services[EB/OL]. [2013-12-21]. http://www.halliburton.com/public/lp/contents/Data_Sheets/web/WPS_ Chapter 6.pdf.
[28] Halliburton Limited. CAST-MTN/CBL-M/MFC[EB/OL]. [2012-10-05]. http://www.halliburton.com/public/lp/contents/Data_Sheets/web/H/H09924.pdf.
[29] WeatherfordLimited.Magnetic-fluxleakageandtransversefieldinspection technologies [EB/OL]. [2013-11-13]. http://www.weatherford.com/weatherford/groups/web/documents/weatherfordcorp/wft089757.pdf.
[30] Weatherford Limited. Casing imaging tool (CIT)[EB/OL]. [2013-04-07]. http://www.weatherford.com/weatherford/groups/web/documents/weatherfordcorp/wft031949.pdf.
[31] Weatherford Limited. Casing imaging tool finds corroded casing section where other methods gail[EB/OL]. [2013-05-03]. http://www.weatherford. com/weatherford/groups/web/documents/weatherfordcorp/wft065486.pdf.

基金

国家科技重大专项(2011ZX05043-003)
PDF(1662 KB)

Accesses

Citation

Detail

段落导航
相关文章

/