Reviews

Review on Casing Corrosion Testing Techniques outside China

  • WANG Lichen ,
  • ZHEN Jian ,
  • ZHU Guiqing
Expand
  • 1. CNPC Economics & Technology Research Institute, Beijing 100724, China;
    2. No. 2 Drilling Company, CNPC Bohai Drilling Engineering Company Limited, Langfang 065007, China

Received date: 2014-02-07

  Revised date: 2014-03-21

  Online published: 2014-07-02

Abstract

Corrosion phenomena are widespread during the process of oil and gas exploration and production. Corrosion prevention and control are necessary in protection of oil-gas exploitation facilities, such as the casing, tubing and wellhead, to guarantee economic and production efficiency. Corrosion testing techniques are important means to deal with corrosion problems with high resolution and good continuity. This paper mainly addresses the casing corrosion problems by introducing the current status and development trend of casing corrosion testing techniques outside China.

Cite this article

WANG Lichen , ZHEN Jian , ZHU Guiqing . Review on Casing Corrosion Testing Techniques outside China[J]. Science & Technology Review, 2014 , 32(18) : 67 -72 . DOI: 10.3981/j.issn.1000-7857.2014.18.011

References

[1] Koch G H, Brongers M P H, Thompson N G, et al. Corrosion cost and preventive strategies in the united states[R/OL]. [2010-02-03]. http://www.corrosioncost.com/home.html.
[2] NACE. Monitoring corrosion in oil and gas production with iron counts[R/OL]. [2011-04-05]. http://www.setlaboratories.com/NACE/tabid/61/Default.aspx.
[3] Brill T M, Calvez J L L, Demichel C, et al. Electromagnetic casing inspection tool for corrosion evaluation[C]. International Petroleum Technology Conference, Bangkok, Thailand, February 7-9, 2012.
[4] Brondel D, Edwards R, Hayman A, et al. Corrosion in the oil industry[J]. Oilfield Review, 1994, 6(2), 4-18.
[5] Lord W, Sun Y S, Udpa S S, et al. A finite element study of the remote field eddy current phenomenon[J]. Magnetics, IEEE Transactions on, 1988, 24(1): 435-438.
[6] Kermani M B, Morshed A. Carbon dioxide corrosion in oil and gas production—A compendium[J]. Corrosion, 2003, 59(8): 659-683.
[7] Li S, Liu C, Shen L. A New 3-D electrode-type logging tool[C]. 2006 SEG Annual Meeting. Society of Exploration Geophysicists, New Orleans, USA, October 1-6, 2006.
[8] 孙喜寿. 井下套管腐蚀监测及评定多层套管柱腐蚀的解释技术[J]. 国 外石油工程,1993(1): 58-64. Sun Xishou. Downhole casing corrosion monitoring and evaluation of the interpretation of the multilayer casing corrosion technology[J]. Foreign oil engineering, 1993(1): 58-64.
[9] 杨旭, 刘书海, 李丰, 等. 套管检测技术研究进展[J]. 石油机械, 2013, 41(8): 17-22. Yang Xu, Liu Shuhai, Li Feng, et al. Research progress in casing detection technology[J]. China Petroleum machinery, 2013, 41(8): 17-22.
[10] 唐宇. 套管井分析技术ABC (Analysis Behind Casing)[J]. 测井技术, 2011, 35(1): 88. Tang Yu. Analysis behind casing[J]. Well logging technology, 2011, 35 (1): 88.
[11] 林俊明. 电磁无损检测技术的现状与发展趋势[C]//中英无损检测技 术研讨会论文集. 上海: 中国机械工程学会, 2005: 42-50. Lin Junming. The current situation and trend of development of electromagnetic nondestructive testing technology[C]//Nondestructive Testing Technology Symposium. Shanghai: Chinese Mechanical Engineering Society, 2005: 42-50.
[12] 关松. 油水井套损检测技术分析与评价[J]. 石油仪器, 2010, 24(2): 64-66. Guan Song. Oil and water wells casing damage detection technology analysis and evaluation[J]. Oil Instrument, 2010, 24(2): 64-66.
[13] 李福军, 陈月勋, 李晓川, 等. 油水井套管的腐蚀及防护理论、实验与 应用—油水井套管的腐蚀与防护[J]. 大庆石油学院学报, 2004, 28 (2): 57-62. Li Fujun, Chen Yuexun, Li Xiaochuan, et al. Corrosion and anticorrosion of casing in oil and water wells[J]. Journal of Daqing Petroleum Institute, 2004, 28(2):57-62.
[14] Zhu G Y, Zhang S C, Liang Y B, et al. Origins of high H2S-bearing natural gas in China[J]. Acta Geol Sinica, 2005, 79(5): 697-708.
[15] Yin Z F, Zhao W Z, Bai Z Q, et al. Corrosion behavior of SM80SS tube steel in stimulant solution containing H2S and CO2[J]. Electrochemica Acta, 2008, 53(10): 3690-3700.
[16] 王军, 毕宗岳, 张劲楠, 等. 油套管腐蚀与防护技术发展现状[J]. 焊 管, 2013, 36(7): 17-22. Wang jun, Bi Zongyue, Zhang Jinnan, et al. Current status of casing/tubing corrosion and protection technology[J]. Welded Pipe and Tube, 2013, 36(7): 17-22.
[17] Brill T M, Calvez J L L, Demichel C, et al. Quantitative corrosion assessment with an EM casing inspection tool[C]. SPE 149069, New Orleans, USA, May 15-18, 2011.
[18] Schlumberger Limited. Casing corrosion measurement to extend asset life[EB/OL]. [2013-10-03]. http://www. slb.com/-/media/Files/resources/oilfield_review/ors13/aut13/2_casing_corr.pdf.
[19] Schlumberger Limited. Scanning for downhole corrosion[EB/OL]. [2013-10-25]. http://www.slb.com/-/media/Files/resources/oilfield_review/ors 10/spr10/04_downholecorrosion.pdf.
[20] Schlumberger Limited. EM pipe scanner brochure[EB/OL]. [2013-07-1 3]. http://www.slb.com/-/media/Files/evaluation/brochures/scanner_rock_ fluid_character/em_pipe_scanner_br.pdf.
[21] Schlumberger Limited. METT multi-frequency electromagnetic thickness tool[EB/OL].[2013-06-09].http://www.slb.com/services/characterization/wireline_cased_hole/corrosion_evaluationmultifrequency_electromagnetic. aspx.
[22] Schlumberger Limited. UCI ultrasonic casing imager[EB/OL]. [2013-11-23]. http://www.slb.com/services/characterization/wireline_cased_hole/corrosion_evaluation/ultrasonic_casing_imager.aspx.
[23] 谢荣华, 刘继生, 张月秋, 等. 检查套管损坏的电磁探伤测井方法及 应用[J]. 测井技术, 2003(3): 69-72. Xie Ronghua, Liu Jisheng, Zhang Yueqiu, et al. Detecting casing damages with electromagnetic defect detection log and its applications[J]. Well logging technology, 2003(3): 69-72.
[24] Baker Hughes Limited. Well integrity service[EB/OL]. [2013-09-14]. http://www.bakerhughes.com/products-and-services/evaluation/casedhole-wireline-systems/well-integrity.
[25] Halliburton Limited. Casing integrity monitoring for mature fields[EB/OL]. [2013-12-11]. http://www.halliburton.com/public/lp/contents/Brochures/web/H010381.pdf.
[26] Halliburton Limited. XaminerTN multicomponent induction (MCI) tool[EB/OL]. [2013-02-08]. http://www.halliburton.com/public/lp/contents/Data_Sheets/web/H/H09310.pdf.
[27] Halliburton Limited. Downhole video services[EB/OL]. [2013-12-21]. http://www.halliburton.com/public/lp/contents/Data_Sheets/web/WPS_ Chapter 6.pdf.
[28] Halliburton Limited. CAST-MTN/CBL-M/MFC[EB/OL]. [2012-10-05]. http://www.halliburton.com/public/lp/contents/Data_Sheets/web/H/H09924.pdf.
[29] WeatherfordLimited.Magnetic-fluxleakageandtransversefieldinspection technologies [EB/OL]. [2013-11-13]. http://www.weatherford.com/weatherford/groups/web/documents/weatherfordcorp/wft089757.pdf.
[30] Weatherford Limited. Casing imaging tool (CIT)[EB/OL]. [2013-04-07]. http://www.weatherford.com/weatherford/groups/web/documents/weatherfordcorp/wft031949.pdf.
[31] Weatherford Limited. Casing imaging tool finds corroded casing section where other methods gail[EB/OL]. [2013-05-03]. http://www.weatherford. com/weatherford/groups/web/documents/weatherfordcorp/wft065486.pdf.
Outlines

/