Tahe Oilfield Gas Pipeline Corrosion Characteristics and Rules

  • ZHANG Jiangjiang
Expand
  • Northwest Oilfield Company, China Petroleum & Chemical Corporation, Urumqi 830011, China

Received date: 2014-06-12

  Revised date: 2014-07-09

  Online published: 2014-11-15

Abstract

Carbonate oilfield in Tahe oilfield for marine sedimentary formation, formation fluid with high salinity, high Cl-, high CO2, high H2S characteristics, and the injection gas well gas injection, soaking and production process, containing dissolved oxygen, make the corrosion environment even worse. Through mining based liquid water analysis, pipeline operation condition analysis and gas injection technology research for gas injection wells of carbonate rock reservoir, analysis, application of XRD diffraction intensity of scanning electron microscope, energy spectrum analysis and point corrosion image analysis VMS test analysis methods, study on the reaction of corrosion products and morphology of downhole and surface pipeline characteristics, through the pipeline in gas injection well tubing downhole, wellhead and Christmas tree and ground production pipeline hang into the three in material for monitoring coupon, to study the gas injection, soaking and production process in different monitoring sites of pipeline's corrosion rate, morphology and rule of law, to: from the bottom, wellhead to the ground pipeline, with the increase of corrosion pit monitoring period, deepen and strengthen, the corrosion rate increased; the process of gas injection, soak process to the process of corrosion degree gradually become larger, longitudinal corrosion capability is strong; gas injection and production process of 35CrMo, P110S and P110 three kinds of pipeline with corrosion resistance material change difference. And the analysis of mechanism model and a gas injection, soaking and production process control of injection well bottom, wellhead and ground pipeline corrosion characteristics and rules.

Cite this article

ZHANG Jiangjiang . Tahe Oilfield Gas Pipeline Corrosion Characteristics and Rules[J]. Science & Technology Review, 2014 , 32(31) : 65 -70 . DOI: 10.3981/j.issn.1000-7857.2014.31.009

References

[1] 曹楚南. 腐蚀电化学原理[M]. 北京: 化学工业出版社, 2004: 55-77. Cao Chunan. The corrosion electrochemistry principle[M]. Beijing: Chemical Industry Press, 2004: 55-77.
[2] 翁永基. 材料腐蚀通论——腐蚀科学与工程基础[M]. 北京: 石油工业 出版社, 2004: 56-80. Weng Yongji. Material corrosion general theory: Corrosion science and engineering foundation[M]. Beijing: Petroleum Industry Press, 2004: 56- 80
[3] 唐世春, 张志宏, 张江江. 塔河油田点蚀测试及评价技术应用[J]. 科技 导报, 2013, 31(32): 42-48. Tang Shichun, Zhang Zhihong, Zhang Jiangjiang. Application of test and evaluation technology of pitting corrosion in Tahe Oilfield[J]. Science & Technology Review, 2013, 31(32): 42-48.
[4] 赵文娜, 王宇宾, 张烨. 高温地面交联酸体系研究及其现场应用[J]. 科 学技术与工程, 2013, 13(8): 2191-2193. Zhao Wenna, Wang Yubin, Zhang Ye. Study and application of the ground cross-linked acid with high-temperature resistance [J]. Science Technology and Engineering, 2013, 13(8): 2191-2193.
[5] 张江江, 刘冀宁. 表面工程应用实例[例33]三元牺牲阳极镀层在油田 管道防腐中的应用[J]. 中国表面工程, 2014, 27(1): F0002. Zhang Jiangjiang, Liu Jining. Surface engineering application examples[Example 33] application of ternary sacrificial anode coating for oilfield pipeline[J]. China Surface Engineering, 2014, 27(1): F0002.
[6] 羊东明, 李亚光, 张江江, 等. 大涝坝气田油管腐蚀原因分析及治理对 策[J]. 石油钻探技术, 2011, 39(5): 81-84. Yang Dongming, Li Yaguang, Zhang Jiangjiang, et al. The corrosion evaluation of inter-station accompanying gas pipeline in Tahe Oilfield[J]. Petroleum Drilling Techniques, 2011, 39(5): 81-84.
[7] 韩阳, 张江江, 羊东明. 清管技术在TH10244单井集输管线中的应用[J]. 中国高新技术企业, 2013(13): 59-60. Han Yang, Zhang Jiangjiang, Yang Dongming. Pigging technology application in TH 10244 pipeline of single well[J]. China High-Tech Enterprises, 2013(13): 59-60.
[8] 中华人民共和国国家质量监督检验检疫总局. GBT18590—2001: 金 属和合金的腐蚀点蚀评价方法[S]. 北京: 中华人民共和国国家质量监 督检验检疫总局, 2001: 3-11. General Administration of Quality Supervision, Inspection and Quarantine of the People's Republic of China GBT18590—2001: Corrosion of metals and alloys- evaluation of pitting corrosion[S]. Beijing: General Administration of Quality Supervision, Inspection and Quarantine of the People's Republic of China, 2001: 3-11.
[9] 张志宏, 张江江, 刘冀宁, 等. 塔河油田腐蚀监测工艺评价及优化[C]// 全国油气田管道腐蚀检测、防护预警技术科技创新技术交流会. 昆 明, 2012. Zhang Zhihong, Zhang Jiangjiang, Liu Jining, et al. Tahe oilfield corrosion monitoring process evaluation and optimization[C]//The national meeting of oil and gas pipeline corrosion detection, protection warning technology innovation and technological exchanges will. Kunming, 2012.
[10] 李效波, 张海龙. 热采筛管冲蚀与腐蚀迭加作用机理[J]. 科技导报, 2014, 32(3): 49-55. Li Xiaobo, Zhang Hailong. Erosion and corrosion superposition mechanism of thermal screen[J]. Science & Technology Review, 2014, 32(3): 49-55.
[11] 张江江, 黄鹏, 高淑红, 等. 超声C扫描检测技术在塔河油田管道检 测中的应用与评价[J]. 化工自动化及仪表, 2013, 40(11): 1355-1359. Zhang Jiangjiang, Huang Peng, Gao Shuhong, et al. Ultrasonic C-scan detection technology for pipe in spection and evaluation intaheoilfield[J]. Control and Instruments in Chemical Industry, 2013, 40(11): 1355- 1359.
[12] 张志宏, 张江江, 高秋英, 等. 塔河油田某侧钻深井油管断裂失效原 因分析[J]. 科技导报, 2014, 32(7): 62-66. Zhang Zhihong, Zhang Jiangjiang, Gao Qiuying, et al. Analysis of rupture failure of sidetrack deep well pipe in Tahe oilfield[J]. Science & Technology Review, 2014, 32(7): 62-66.